The compacted magnets are sintered at temperatures above 1000 centigrade and for many hours to be solidified and compacted further more up to 99% by shrinking it's body. A required microstructure between particles for high performance permanent magnets is also formed in this stage. Some following heat-treatments are needed to stabilize the magnets .